Application
Used For Cast Iron, Malleable Steel, Galvanized Steels, Brass and Copper
Brazing Range (F)
1595 to 1630
Tensile Strength (PSI)
80 to 98
For Joining
Cast Iron to Copper, Cast Iron to Stainless Steel, Cast Iron to Steel, Copper to Stainless Steel, Copper to Steel, Stainless Steel to Steel, Steel to Steel
Flux Application
Flux Required for Cast Iron to Cast Iron, Flux Required for Cast Iron to Copper, Flux Required for Cast Iron to Stainless Steel, Flux Required for Cast Iron to Steel, Flux Required for Copper to Stainless Steel, Flux Required for Copper to Steel, Flux Required for Stainless Steel to Steel, Flux Required for Steel to Steel
Joining Applications
Cast Iron to Cast Iron, Cast Iron to Copper, Cast Iron to Stainless Steel, Cast Iron to Steel, Copper to Stainless Steel, Copper to Steel, Stainless Steel to Steel, Steel to Steel
Capacity Shingles
1,750 Degrees F
Compatible Chuck Size
1,670 Degrees F
Brazing Temperature Range
1,670 Degrees F to 1,750 Degrees F
AWS Classification
RBCuZn-C
Alloy Type
Low-Fuming Bronze
Alloy Composition
56% to 60% Copper, 0.8% to 1.1% Tin, 0.25% to 1.2% Iron, 0.01% to 0.5% Manganese, 0.05% Lead, 0.04% to 0.15% Silicon, 0.01% Aluminum, 0.5% Other, Balance Zinc
For Metal Type
Cast Iron to Cast Iron, Cast Iron to Copper, Cast Iron to Stainless Steel, Cast Iron to Steel, Copper to Stainless Steel, Copper to Steel, Stainless Steel to Steel, Steel to Steel
Maximum Brazing Temperature
1,750 Degrees F
Minimum Brazing Temperature
1,670 Degrees F
Minimum Soldering Temperature
1,670 Degrees F
Country of Origin (subject to change)
China